"A supplier's guide to 1,4-cyclohexanedimethanol (CAS 105-08-8): cis/trans ratio, 31.5C melting point, PETG and powder coating uses, UV-cure routes, safe storage and what to check on a COA before ordering."

-Deshangchemical-chemechemi

A diol that changes state near room temperature

Buyers who search for 1,4-cyclohexanedimethanol (CAS 105-08-8) usually know what they want it for. The material is a saturated cycloaliphatic diol, C8H16O2, molecular weight 144.21, EINECS 203-268-9, with one hydroxymethyl group at each end of a cyclohexane ring. It is also written as CHDM or 1,4-cyclohexane dimethanol. Our listing describes an off-white, faintly odorous waxy solid. Typical sheet data: melting point 31.5 °C, boiling point 283 °C, density 1.04 g/cm3, refractive index around 1.424, flash point 322 °F, vapor pressure 0.24 Pa at 20 °C, water solubility above 34 g/L and a predicted pKa of 14.75. Storage below 30 °C follows from that melting point.

That 31.5 °C line is the first practical detail in any order. A drum stored in a warm warehouse can arrive as a softened mass or a solid block rather than free-flowing flakes, and that is normal behavior, not a quality claim. Warm the drum gently, let the whole lot reach the same temperature and mix before sampling or charging. Drawing from a partly melted drum without mixing gives a misleading assay on the first sample and a different one on the last.

The cis/trans ratio belongs on the specification

Commercial CHDM is not a single stereoisomer. At equilibrium the product is roughly 24% cis and 76% trans. The two forms behave differently in a polyester chain: the trans isomer packs more regularly, so trans-rich grades crystallize more readily and give higher glass transition temperature and hardness; the cis isomer disrupts packing and slows crystallization. If your process depends on how fast a pellet crystallizes or how clear a sheet stays after thermoforming, "CHDM, 99%" is not enough information. Ask for the isomer ratio on the COA.

The ratio is normally measured by gas chromatography, commonly with an SE-54 or polyethylene glycol 20M capillary column and a flame ionization detector under programmed temperature. The same method also checks assay. When you compare offers, a supplier quoting only purity and appearance may be offering a different cis/trans balance, and that can explain the price gap. For a long-term contract, fix the ratio range in writing rather than relying on a catalogue average.

PETG and modified PET are the volume outlets

CHDM is best known as the comonomer in PETG. In practice a polyester producer replaces part of the ethylene glycol in the polycondensation with CHDM while keeping terephthalic acid (PTA) as the diacid. The cyclohexane ring breaks up the regularity of the PET chain, slows crystallization and helps the polymer stay clear through thermoforming. That is why PETG turns up in transparent sheet for blister packaging, retail display, clear food containers, bottles and optical film where clarity has to survive thermoforming. Isophthalic acid is often discussed in the same breath, but it changes the chain in a different way and is chosen for a different balance of properties.

Even small additions of CHDM to standard PET change the crystallization window and raise the glass transition temperature. That can be useful for hot-fill containers and for films that must withstand heat, but it also means existing cooling and stretching settings may need adjustment. Run a trial on the production line, not only in a lab oven. Where the target is simply a more flexible, lower-crystallinity polyester without the cycloaliphatic ring, neopentyl glycol is the alternative diol buyers compare against. Neither is a drop-in replacement; state the target Tg and clarity when asking for a quote.

Powder coatings reward the trans-rich grade

A large share of CHDM goes into saturated polyester resins for powder coatings. Trans-rich CHDM polyesters offer the hardness, glass transition temperature and weatherability that exterior finishes need, including automotive clearcoats, architectural aluminum, appliance panels and general industrial topcoats. Resin makers control acid value and hydroxyl value to set the crosslink density with the curing agent, and the isomer balance of the diol is one of the levers they use to hit those numbers.

On the synthesis side, esterification and polycondensation are typically catalyzed by tin or titanium compounds; titanium tetraisopropanolate is one of the organotitanium options in our range. For outdoor exposure, a hindered amine light stabilizer or a UV absorber such as benzotriazole usually sits in the topcoat rather than in the resin itself. Asking which of these your resin supplier already uses avoids adding a package that duplicates what is in the system.

Unsaturated resins, polyols and radiation curing

In unsaturated polyester resins, CHDM can raise hardness, gloss and weather resistance in gelcoats, glass-fiber reinforced parts and sheet molding compounds. The diacid side of that formulation may be adipic acid, or an ester such as dimethyl glutarate and dimethyl azelate depending on the flexibility required. CHDM-derived polycarbonate diols also start polyurethane elastomers for abrasion- and chemical-resistant parts.

Another route goes through polycaprolactone. Caprolactone polymerizes to polycaprolactone polyols for polyurethane systems, and caprolactam is the nylon 6 monomer. They share a ring size with nothing else in this story: CHDM is a diol, not a lactone or a lactam, and substituting one for another is not a formulation decision.

Alkoxylated CHDM acrylates are used in radiation-cured coatings and inks, where they cure quickly and leave a flexible film. Formulators pair them with reactive monomers such as hydroxyethyl acrylate or polyethylene glycol diacrylate, and with non-reactive carriers including dipropylene glycol and polypropylene glycol. CHDM itself is not a low-viscosity diluent: the listed viscosity is 675 mPa·s at 50 °C, so heated handling and metering are part of the process where neat material is charged.

Solubility, storage and safety notes

CHDM mixes with water and lower alcohols and dissolves in ketone solvents, while solubility in aliphatic hydrocarbons and ethers is very low. Use that when you design a cleaning step or a solvent blend; a wash that works for a polar diol may leave residue in a hydrocarbon-rich system. Keep containers closed and stored below 30 °C, away from heat sources and oxidizers. The material is combustible and heated decomposition gives off irritating smoke, so ventilation, gloves and eye protection are standard practice. Check the current SDS before writing the site procedure.

Do not confuse CHDM with 1,4-cyclohexanediol, where the hydroxyl groups sit on the ring rather than on hydroxymethyl arms. The two have different melting behavior and reactivity in polycondensation. Match any drawing that says CHDM back to CAS 105-08-8.

What to put in the inquiry

State the polymer system and the property you are chasing, whether clarity after thermoforming, a target Tg for powder coating resin, or hydrolysis resistance in a polyurethane. Ask for GC assay, cis/trans ratio, melting range, color, water content, acid value and residual solvent on the COA. Confirm the physical form and packing, since flakes and a warmed liquid ship differently, and say whether the grade is for polyester resin, coating or intermediate use. For food-contact packaging, request compliance documents up front. A sample tested in your own process tells you more than extra catalogue numbers, and the isomer ratio is the column worth reading first.

Get a free quote!


+86-531-88752665